The production of the insulation bottle seems simple but there are many links. The negligence of any link may cause the lack of the appearance or function of the water bottle/tumbler. In production, Ailin requires workers to follow strict standard processes to operate, and do their best to improve the pass rate.

The thermal water bottle is composed of an inner tank, a vacuum layer and an outer shell. Different structures are manufactured by different processes and cooperate with each other.

Cut tube

Sharpen

Hydroforming

Laser cutting

Shrinking

Welding cup mouth

Welding outsole

Vacuuming

Vacuum test

Sharpening & polishing

Painting & printing

Packing

Tube cutting

Use a lathe, specifically in accordance with the “Instructions for Cutting Pipes”, which requires accurate dimensions, timely detection of defective products and waste materials, and avoid pits, pits, pits, and scrap products during operation.

Water swelling

The water expansion press shall be implemented according to the “Water Expansion Operation Instruction”, requiring concentration and always paying attention to whether the product’s pits, size, and shape meet the requirements.

Divide the tube

Use an instrument car to cut off the two shells that have swelled from one to the other. It is required to have accurate dimensions, uniform cuts, no gaps, and burrs. Handle with care to avoid pits, pits, pits, and scrapped products.

Cut the bottom

Use a lathe to cut the bottom of the shrunk shell to the standard size. The cut is uniform, without gaps, and burrs. Handle with care to avoid pits, pits, pits, and scrapped products.

Flat the mouth and the bottom

Use a lathe, the flat opening is even, without gaps, and burrs, which meets the requirements. Handle with care to avoid pits, pits, pitting, and scrapped products.

Rolling thread

Use a special threading machine, specifically in accordance with the “Thread Rolling Operation Instructions”, requiring concentrated attention, adjusting the thread depth to meet the size requirements; handle with care to avoid pits, pits, pitting, and scrap products.

Rolling the mouth

Use a lathe to roll the protruding corner of the bulged liner to meet the size requirements, handle it with care, and avoid pits, pits, pitting, and scrapped products.

Washing and drying

Clean and dry the liner and shell; handle with care to avoid pits, pits, pitting, and scrapped products.

Knock on the recessed point

Check whether the inner tank and outer shell are qualified, and if there are pits and pits, knock them flat to meet the requirements, and handle them with care.

Circumferential welding

Weld the bottom of the inner to the inner tank

 

Welding mouth and bottom

Specifically, it shall be implemented in accordance with the “Operation Instructions for Welding Joint Welding Process”, and it is required to ensure that the bottom of welding joint is penetrated and smooth, without concave and convex points, welding tumors and missing solder joints.

Welding getter

The getter is spot welded on the midsole. Note that the getter on the spot welding must be vacuumed within 24 hours, otherwise it will be invalid.

Press the midsole: press the welded cup onto the midsole where the getter is spot welded, and the pressure is even with the bottom.

Vacuumize

Tailless vacuuming, strictly in accordance with the vacuuming operation standard.

Thermometry

Specifically follow the “Operation Instructions for Electric Temperature Measurement Process”, check whether the cup is vacuum, and pick out the non-vacuum cup.

Electrolysis

Send out the electrolysis to the external association, and the electrolysis in the cup is required to be bright and even, without watermarks and yellow spots.

Паліроўка

The shell of the cup is required to be polished finely and the lines are orderly, the mouth of the cup is smooth and bright, and there should be no obvious drawing, scratches, black threads and pits, and residual polishing paste.

Press outsole

press the outsole on the polished cup to make it flat.

Surface process

Spray paint or plastic spraying, pattern making and other processes on the embryo body.

Leak test

Inflate the welded liner to test the water, and check whether there are any loopholes in the welding seam, and it is qualified if there is no leakage.

Matching mouth

Put the liner and shell together, and make the cup mouth flat; handle with care to avoid pits, pits, pitting, and scrapped products.

Tube cutter

Automatic shrinking machine

Mating welding machine

Temperature measuring machine